de Cezar Popescu | oct. 20, 2011 | Developers, Tanning developers
Tanning developer for color separation positives (dye-tone process). IngredientQuantity Sodium sulphite anhydrous50grams Pyrocatechin20grams Sodium carbonate anhydrous100grams Potassium bromide4grams Water to make1liter Mix chemicals in order. Dilute 1:5 and develop...
de Cezar Popescu | oct. 20, 2011 | High acutance developers
Soft working developer designed for color separation negatives. IngredientQuantity Sodium sulphite anhydrous50grams Glycin9grams Kodalk40grams Water to make1liter Mix chemicals in order. For tray processing pre-soak the film for 2 minutes in plain water. Do not dilute...
de Cezar Popescu | oct. 20, 2011 | High contrast developers
High contrast MQ developer. IngredientQuantity Metol1gram Sodium sulphite anhydrous75grams Hydroquinone9grams Sodium carbonate anhydrous25grams Potassium bromide5grams Water to make1liter Mix chemicals in order. Do not dilute. Develop 5–10 minutes at 18.5°C. For less...
de Cezar Popescu | oct. 20, 2011 | High contrast developers
High contrast developer for films. IngredientQuantity Solution A Sodium bisulphite22.5grams Hydroquinone22.5grams Potassium bromide22.5grams Solution B Sodium hydroxide52.5grams Cold water to make1liter Mix chemicals in order. The sodium hydroxide should not he...
de Cezar Popescu | oct. 20, 2011 | General purpose developers, High contrast developers
Glycin hydroxide developer for tray use. IngredientQuantity Sodium sulphite5grams Sodium hydroxide16grams Glycin4grams Water to make1liter Mix chemicals in order. For very badly underexposed negatives or for strong contrast, use full strength. For softer negatives,...